In-house master pattern production
SLA and CNC machining for high-accuracy masters before casting.
Vacuum casting produces small series of plastic parts using silicone molds made from a master pattern. The master (typically produced by SLA or CNC machining) is used to cast a silicone mold. Liquid polyurethane resin is cast into the mold under vacuum, eliminating air bubbles and reproducing fine surface detail.
Each silicone mold yields 20-25 parts before requiring replacement. The process is suitable for small series requiring surface quality and material properties close to injection molding, without the cost of hard tooling.
SLA and CNC machining for high-accuracy masters before casting.
7-14 days from approved design to delivery.
No hard tooling investment required.
30+ PU resin types simulating ABS, PP, PC, rubber, and engineering elastomers.
Cast polyurethane parts in silicone molds at surface quality close to injection-molded parts. Suitable for appearance prototypes, functional testing, and bridge production before tooling.
Water-clear PU resins produce optically transparent parts. Suitable for lens covers, display windows, light guides, and aesthetic components where clarity matters.
Rigid and flexible resins combined in one part. Suitable for soft-grip handles, two-material enclosures, and ergonomic assemblies.
Custom textures applied to the silicone mold replicate leather grain, surface patterns, or fine detail. Suitable for consumer products, automotive interior trim, and ergonomic parts.
Step 1
A high-accuracy master is produced by SLA 3D printing or CNC machining.
Step 2
The master is suspended in a mold box and liquid silicone poured around it; cured for 8-16 hours.
Step 3
PU resin is chosen to match the target mechanical properties and surface finish.
Step 4
Resin is poured into the mold under vacuum and cured at 60°C.
Step 5
Cast part removed after curing; gates and flashing trimmed.
Step 6
Paint, primer, or surface treatment applied if required. Parts inspected and shipped.
| Material | Key Properties | Suitable Applications |
|---|---|---|
| ABS-like PU | Rigid, good impact resistance, sandable | Housings, brackets, functional prototypes |
| PP-like PU | Slightly flexible, living-hinge capable | Clips, caps, snap-fit components |
| PC-like PU | High impact, heat resistant | Enclosures, structural housings, covers |
| Rubber-like PU (Shore A 40-80) | Flexible, elastic, tear resistant | Seals, grips, overmolded soft components |
| Nylon-like PU | Tough, slightly flexible | Snap fits, gears, load-bearing functional parts |
| Transparent PU | Optically clear, scratch resistant | Lenses, windows, display covers |
| High-Temp PU (HDT >120°C) | Heat resistant | Under-hood parts, heat-exposed components |
| Glass-Filled PU | Higher stiffness than standard PU | Structural brackets, dimensionally stable parts |
Typical tolerance: ±0.3mm on standard geometries
Maximum part size: 800 x 500 x 400mm (master pattern dependent)
Parts per mold: 20-25 pieces per silicone mold
Lead time: 7-14 business days from approved design
Minimum order: 1 piece
Surface finish: A1-A3 gloss (SLA master), B1-B2 fine matte (machined master); texture available on request
Available post-finishes: primer, paint, chrome-effect lacquer, matte, gloss
Automotive
Consumer Products
Medical and Life Sciences
Consumer Electronics
Industrial Equipment
Vacuum casting delivers production-like parts without tooling investment. Quote within 24 hours.