DefinitionAn undercut is any feature on a molded part that prevents it from being pulled straight out of the mold in the direction the mold opens, such as a side hole, snap-fit hook, internal groove or thread.
Explained
An undercut is any feature on a molded part that prevents it from being pulled straight out of the mold in the direction the mold opens, such as a side hole, snap-fit hook, internal groove or thread. Undercuts need extra mold mechanisms—usually side actions or lifters—or a design change so the part can release.
What Does Undercut Mean in Injection Molding?
A basic two-plate mold opens in one straight line, the line of draw. Every surface of the part must be able to slide away from the steel along that line. A feature that sits "under" another surface when viewed from the draw direction, such as a hole through a side wall or a latch that hooks sideways, would be trapped by the mold and torn off or jammed on ejection.
Undercuts are not a design mistake in themselves. Snap fits, side ports, threads and clips are often exactly what a part needs. The question is how the mold will release them.
How Are Undercuts Molded?
There are five common ways to mold undercuts, each with different tooling impacts:
- Redesign with a shut-off: Reshape the feature so the core and cavity meet through it, often with a slot or opening in the opposite wall. Best for simple latches and snap hooks; no added tooling cost.
- Side action (slide): A core pulls sideways out of the feature before the part is ejected, driven by angled cam pins or its own actuator. Best for holes and features on outside walls; adds a moving component and cost.
- Lifter: An angled core moves with the ejector system, sliding sideways off the feature as the part is pushed out. Best for internal clips and undercuts inside a wall; adds cost and needs room behind the feature.
- Hand-loaded insert: A loose insert is molded in, removed with the part and pulled out by hand. Best for prototype and low-volume tools; low tool cost but slower cycle.
- Stripping (bump-off): The part flexes over a shallow undercut during ejection. Only works with forgiving materials and small depths.
How to Design Around Undercuts
- Check every feature against the draw direction early; many undercuts disappear if the parting line or pull direction is chosen differently.
- Ask whether the feature can face the draw direction.
- Group side features on the same face so one side action can form several of them.
- Allow room for side actions and lifters, including a clear travel path.
- Keep mechanisms only for features that earn them; each side action adds cost, maintenance and sometimes cycle time.
Undercuts are one of the items a DFM review is designed to catch before tooling starts.
Key takeaways
- Undercuts are features that prevent a molded part from being ejected straight out of the mold.
- Common examples include side holes, snap-fit hooks, internal grooves and threads.
- Undercuts can be released using shut-offs, side actions, lifters, hand-loaded inserts or stripping.
- Each side action or lifter adds tooling cost, maintenance and sometimes cycle time.
- A DFM review should catch undercuts before tooling starts.
Example
Related terms
References
- Part 4: Injection Mold Design — Texas A&M University (Richland College injection molding curriculum)
- US Patent 6,116,891 — Google Patents
- US Patent 5,137,442 — Google Patents